Aluminium Alloys for CNC Machining: Series, Properties, Selection
Updated
Aluminium alloys are the most commonly CNC-milled material: they are light (about 2.7 g/cm³), machine well at high speeds and can be anodised. General-purpose parts usually use 6082 or 6061 T6, high-strength parts 7075 T6, plates and marine applications 5083, and free-machining turned parts 2xxx-series alloys.
Aluminium alloys are aluminium-based metals alloyed with copper, magnesium, silicon, zinc or manganese to increase strength, hardness or corrosion resistance. In CNC production they are the most popular material family: aluminium machines several times faster than steel, causes little tool wear and finished parts can be anodised. Under ISO 513 aluminium belongs to group N – see ISO material groups.
Wrought alloy series
Wrought (rolled, extruded, forged) alloys carry a four-digit number under EN 573 and the international registration. The first digit indicates the main alloying element.
| Series | Main element | Heat treatable | Typical alloys | Machinability |
|---|---|---|---|---|
| 1xxx | Pure Al (≥99 %) | No | 1050, 1070 | Poor – soft, gummy |
| 2xxx | Copper | Yes | 2017A, 2024, 2007 | Very good |
| 3xxx | Manganese | No | 3003 | Moderate |
| 5xxx | Magnesium | No | 5083, 5754 | Moderate–good |
| 6xxx | Magnesium + silicon | Yes | 6082, 6061, 6060 | Good (in T6) |
| 7xxx | Zinc | Yes | 7075, 7020 | Very good |
Typical properties
| Alloy and temper | Density, g/cm³ | Tensile strength Rm, MPa | Hardness, HB | Machinability |
|---|---|---|---|---|
| 6060 T6 | ~2.70 | ~190–240 | ~65–75 | Good, long chips |
| 6082 T6 | ~2.70 | ~290–340 | ~90–100 | Good |
| 5083 H111 | ~2.66 | ~270–350 | ~70–80 | Moderate, gummier |
| 2017A T4 / T451 | ~2.79 | ~390–430 | ~105–115 | Very good |
| 7075 T6 / T651 | ~2.81 | ~500–570 | ~140–160 | Very good |
Values are typical and depend on product form and thickness; exact limits are given in EN 485 (sheet, plate), EN 755 (extruded bar and profiles) and the supplier's certificate.
Tempers
- T6 – solution treated and artificially aged; highest strength in 6xxx and 7xxx series.
- T651 – T6 plus controlled stretching to relieve stress; plates distort less when milled.
- T4 / T451 – naturally aged, typical for the 2xxx series.
- O – annealed, soft, machines poorly (gummy chips).
- H111, H32 – tempers of non-heat-treatable alloys (5xxx).
More in heat treatment.
Machining tips
- Tools. Use sharp 2–3 flute carbide end mills with a high rake angle and polished flutes. Uncoated, DLC or ZrN coatings work well; TiAlN-type coatings are generally avoided on aluminium because of adhesion. See tool coatings.
- Cutting speed. With carbide typically from several hundred to over 1000 m/min, usually limited by spindle speed. These are starting values – follow the tool manufacturer's data and the cutting speed calculation.
- Avoiding built-up edge. Too low a feed per tooth causes rubbing and aluminium welding to the edge. A higher fz with good chip evacuation is better.
- Coolant. Emulsion or minimum quantity lubrication (MQL); air blast helps clear chips from pockets.
- Distortion. For thin walls and plates choose T651, leave an even allowance and machine symmetrically.
- Anodising. The 6xxx series anodises best; 2xxx and 7xxx can show uneven colour. See anodizing.
Semi-finished products and casting alloys
Wrought alloys are supplied as extruded bar and profiles, rolled plate and sheet, and forgings. Bar and profile properties are governed by EN 755, plate and sheet by EN 485. Plate is usually more accurate in thickness and lower in residual stress when supplied in T651 or as cast and machined precision plate. Casting alloys are designated EN AC (e.g. AlSi10Mg, AlSi7Mg) and are used for complex housings that are only finish-machined on CNC machines. Silicon-bearing castings are more abrasive, so carbide tools wear faster, and with high silicon content (about 12 % or more) PCD tools are commonly used. The same silicon alloys are used in metal 3D printing, after which parts are often finish-milled.
Common mistakes
- Ordering an "aluminium" part without stating the alloy and temper – these decide strength, price and anodising result.
- Milling thin features from soft (O temper) material – the surface tears and dimensions are unstable.
- Cutting with too low a feed and a cutter with too many flutes – chips pack the flutes.
How to choose an alloy
- General structural parts, housings, brackets – 6082 or 6061 T6.
- High strength, aerospace, sports equipment, moulds – 7075 T6/T651.
- Marine environments, welded structures, plates – 5083.
- High-volume turning, threaded parts – 2017A, 2024 or 2007.
Aluminium milling and turning services can be found on the CNC Pasaulis marketplace.
Frequently asked questions
Which aluminium alloy is best for CNC milling?
For most parts 6082 or 6061 T6 offer good machinability, price and anodising quality; for higher strength 7075 is chosen.
Why does aluminium stick to the end mill?
Soft aluminium welds to the edge when the tool is dull, feed is too low, the coating is unsuitable or coolant is lacking; sharp polished cutters and a higher feed help.
What do T6 and T651 mean?
T6 is the solution-treated and artificially aged temper; T651 is the same temper with additional stretching to relieve internal stress.
Do all aluminium alloys anodise well?
No. The 5xxx and 6xxx series anodise best, while 2xxx and 7xxx often take an uneven or darker colour because of copper and zinc.
What is the density of aluminium?
Most wrought aluminium alloys have a density of about 2.6–2.8 g/cm³, roughly one third of steel.
Looking for someone to do this job? Find a manufacturer on the marketplace or post a request.
Services offered I need a service