6061 and 6082 are heat-treatable Al-Mg-Si alloys and the most popular general-purpose aluminium grades for CNC machining. In the T6 temper their tensile strength is about 290–340 MPa, and they machine, anodise and weld well. 6082 is more common in Europe and slightly stronger, while 6061 is the standard choice in North America and Asia.

Aluminium 6061 and 6082 are 6xxx-series wrought aluminium alloys, alloyed with magnesium and silicon and strengthened by heat treatment (solution treatment and ageing). They are the workhorses of CNC production: housings, brackets, plates, machine frames, prototypes and hundreds of other parts are made from them. Both offer a good balance of strength, machinability, corrosion resistance and cost.

Designations and composition

Parameter60616082
EN designationEN AW-6061 (AlMg1SiCu)EN AW-6082 (AlSi1MgMn)
W.Nr.3.32113.2315
UNSA96061A96082
Mg, %0.8–1.20.6–1.2
Si, %0.4–0.80.7–1.3
Other characteristic elementsCu 0.15–0.40; Cr 0.04–0.35Mn 0.40–1.0

Mechanical and physical properties (T6)

Property6061 T66082 T6
Density~2.70 g/cm³~2.70 g/cm³
Tensile strength Rm~290–320 MPa~300–340 MPa
Yield strength Rp0.2~240–280 MPa~250–310 MPa
Hardness~90–100 HB~90–100 HB
Young's modulus~69 GPa~70 GPa
Thermal conductivity~150–170 W/(m·K)~150–170 W/(m·K)
MachinabilityGood in T6Good in T6

Exact minimum values depend on product form and thickness (EN 755, EN 485) – always refer to the supplier's certificate.

How 6061 and 6082 differ

  • Availability. In Europe bar, extrusions and plate are most often supplied in 6082; in North America and Asia in 6061. In practice they are often interchanged where the drawing permits.
  • Strength. Thanks to higher silicon and manganese, 6082 is usually slightly stronger, particularly in thicker sections.
  • Surface. 6061 often gives a slightly more uniform decorative anodised finish, although both anodise well.
  • Welding. Both can be TIG and MIG welded, but strength in the heat-affected zone drops to roughly T4 level.

Machining tips

  • Temper. Choose T6, or T651 for plate. Annealed (O) or T4 material is softer and forms long, gummy chips.
  • Cutters. 2–3 flute carbide end mills with polished flutes; fewer flutes for deep slots so chips have room. For soft aluminium and plastics single-flute end mills are sometimes used.
  • Cutting data. A typical starting cutting speed with carbide is several hundred m/min or more; feed per tooth for a 6–12 mm cutter is often about 0.03–0.10 mm. These are guide values only; the tool manufacturer's data takes priority. See cutting speed and RPM.
  • Turning. 6082 tends to form long chips, so use inserts with an aluminium chip breaker and adequate feed.
  • Drilling and tapping. Use polished high-helix twist drills; for threads use forming taps or taps designed for aluminium.
  • Distortion. For large pockets leave an even allowance, rough from both sides and take the finishing pass after stresses have relaxed.

Tolerances and surface finish

With 6061 and 6082 T6, tolerances of ±0.05 mm are routinely achieved without special measures, and ±0.01–0.02 mm in stable conditions with a finishing pass. The main factors are temperature (aluminium's thermal expansion is about 23 µm/(m·K), roughly twice that of steel), residual stress and workholding. Precision parts should be measured after they have cooled to room temperature. Milling with sharp polished cutters typically gives Ra 0.8–3.2 µm; a small radial engagement and high spindle speed improve the finish. See surface roughness. Before anodising, remember that the anodic layer changes dimensions: with hard anodising roughly half of the layer thickness grows outward, so precision bores and threads need an allowance or masking.

Typical applications

  • Machine-building parts, mounting plates, brackets, guides.
  • Electronics enclosures and heat sinks.
  • Pneumatic and automation components.
  • Prototypes and one-off parts that are later anodised.

How to choose

For a versatile, readily available and anodisable material choose 6082 T6 (in Europe) or 6061 T6. If you need more than ~350 MPa, consider 7075. If the part will be permanently in seawater or the best weldability without heat treatment is needed, consider 5083. Machining services for 6061 and 6082 can be found on the CNC Pasaulis marketplace.

Frequently asked questions

Can 6061 be replaced with 6082?

In most cases yes, because their T6 properties are very close, but the substitution should be agreed with the customer, especially for critical structures.

Which is stronger, 6061 or 6082?

6082 T6 usually has slightly higher tensile and yield strength than 6061 T6, particularly in thicker products.

Does 6082 anodise well?

Yes, both 6082 and 6061 anodise well, although 6060 or 6061 are sometimes preferred for decorative anodising because of a more uniform colour.

Can 6082 T6 be welded?

Yes, it can be TIG and MIG welded, but strength drops in the heat-affected zone, which must be considered in design.

What is the hardness of 6061 T6?

6061 T6 typically has a hardness of about 90–100 HB.