Stainless Steel 304 and 316 (1.4301, 1.4404): Properties and Machining
Updated
304 (1.4301) and 316 (1.4401/1.4404) are the most common austenitic stainless steels; 316 additionally contains about 2–2.5 % molybdenum and resists chlorides better. They are harder to machine than carbon steel because they work-harden, conduct heat poorly and tend to smear, so sharp tools, constant feed and generous coolant are essential.
Stainless steels 304 and 316 are austenitic chromium-nickel steels containing about 17–19 % chromium and 8–13 % nickel. Chromium forms a thin passive oxide layer that protects against corrosion. Under EN 10088 these grades are designated 1.4301 (304) and 1.4401/1.4404 (316/316L). They account for the majority of all CNC-machined stainless parts.
Designation and equivalents
| EN number | EN name | AISI | UNS | Feature |
|---|---|---|---|---|
| 1.4301 | X5CrNi18-10 | 304 | S30400 | base grade |
| 1.4307 | X2CrNi18-9 | 304L | S30403 | low carbon, better weldability |
| 1.4305 | X8CrNiS18-9 | 303 | S30300 | sulphur added, easiest to machine |
| 1.4401 | X5CrNiMo17-12-2 | 316 | S31600 | ≈ 2–2.5 % Mo |
| 1.4404 | X2CrNiMo17-12-2 | 316L | S31603 | low-carbon 316 |
| 1.4571 | X6CrNiMoTi17-12-2 | 316Ti | S31635 | titanium-stabilized |
In German practice 304 is often called V2A and 316 V4A. See material designation equivalents.
Properties
| Property | 304 / 1.4301 | 316L / 1.4404 |
|---|---|---|
| Density | ≈ 7.9 g/cm³ | ≈ 8.0 g/cm³ |
| Tensile strength Rm (annealed) | ≈ 500–700 MPa | ≈ 500–700 MPa |
| Yield strength Rp0.2 | ≥ ≈ 190–210 MPa | ≥ ≈ 200 MPa |
| Hardness (annealed) | ≈ 150–215 HB | ≈ 150–215 HB |
| Magnetism | annealed – practically non-magnetic; cold-worked can become slightly magnetic | |
| Machinability | harder than carbon steel | slightly harder than 304 |
Austenitic grades cannot be hardened by heat treatment – strength is increased only by cold working. When high hardness and corrosion resistance are needed together, precipitation-hardening 17-4PH is used.
304 or 316?
304 suits most environments: food processing, household equipment and indoor structures. Thanks to molybdenum, 316 resists pitting in chloride environments better – sea water, salt solutions, swimming pools, chemical and pharmaceutical equipment. The L grades (304L, 316L) have ≤ 0.03 % carbon and resist intergranular corrosion after welding.
Machinability
Under ISO 513, austenitic stainless steels belong to group M (ISO material groups). The main challenges are:
- Work hardening. When the edge rubs instead of cutting, the surface hardens and the next pass becomes harder.
- Low thermal conductivity. Heat concentrates in the cutting edge, accelerating wear.
- Smearing. The material tends to weld to the edge and form a built-up edge.
- Long, tough chips, especially in turning.
| Operation (coated carbide) | Vc, m/min | Feed |
|---|---|---|
| Turning | 120–220 | f ≈ 0.1–0.3 mm/rev |
| Milling with an end mill | 80–160 | fz ≈ 0.03–0.10 mm |
| Drilling with a carbide drill | 40–80 | f ≈ 0.08–0.2 mm/rev |
| Tapping (HSS-E tap) | 5–15 | per pitch |
These are typical starting values; the tool manufacturer's data takes priority. See cutting speed and RPM.
Practical tips
- Cut, don't rub. Never let the tool dwell, and do not reduce feed too far – too light a feed work-hardens the surface.
- Sharp, positive-rake tools with inserts and coatings designed for group M (e.g. TiAlN, AlCrN – see tool coatings).
- Generous coolant – flood emulsion or through-tool coolant; this is especially important for drilling and tapping.
- Rigidity. Stable workholding and short tool overhang reduce vibration.
- Threading: use taps designed for stainless steel with good tapping oil, or thread milling (taps).
- If the part will not be welded and involves a lot of turning, consider 1.4305 (303), which machines much more easily but has lower corrosion resistance.
- After machining, the surface can be passivated to restore the protective layer, especially if carbon steel tools or brushes were used.
Typical uses
Food and beverage equipment, pharmaceutical and medical equipment, marine fittings, pump and valve parts, fasteners, flanges, housings, architectural parts and laboratory equipment.
How to choose
- General purpose, food industry – 304 / 1.4301.
- Chlorides, marine environment, chemicals – 316L / 1.4404.
- Lots of turning, no welding, moderate corrosion exposure – 303 / 1.4305.
- High strength or hardness required – 17-4PH / 1.4542.
Machining services for stainless steel parts can be found or requested on the CNC Pasaulis marketplace.
Frequently asked questions
What is the difference between 304 and 316 stainless steel?
316 contains about 2–2.5 % molybdenum and more nickel, which makes it more resistant to pitting in chloride environments such as sea water. Mechanical properties are similar.
What does the L in 316L mean?
L stands for low carbon (≤ 0.03 %), which reduces chromium carbide formation during welding and the risk of intergranular corrosion.
Why is stainless steel hard to machine?
Austenitic stainless steel work-hardens, conducts heat poorly and tends to stick to the cutting edge. Tools wear faster, and slow or rubbing cuts harden the surface.
Is 304 stainless steel magnetic?
Annealed 304 is practically non-magnetic, but after cold working such as bending or drawing it can become slightly magnetic.
Can 304 or 316 be hardened?
No. Austenitic stainless steels cannot be hardened by heat treatment; their strength increases only through cold working.
What is 1.4305 (303)?
It is a variant of 304 with added sulphur, which improves chip breaking and machinability but reduces corrosion resistance and weldability.