Titanium Ti6Al4V (Grade 5): Properties and Machining

Updated

In short

Ti6Al4V (Grade 5, EN 3.7165, UNS R56400) is the most widely used alpha-beta titanium alloy, containing about 6 % aluminium and 4 % vanadium. It combines low density (about 4.43 g/cm³), high strength and excellent corrosion resistance, but is difficult to machine because of its low thermal conductivity and chemical reactivity with tools. It is machined at low cutting speeds with sharp carbide tools and generous coolant.

Ti6Al4V (also written Ti-6Al-4V, Grade 5, EN 3.7165, UNS R56400) is an alpha-beta titanium alloy that accounts for the majority of machined titanium worldwide. It is used where a high strength-to-weight ratio, corrosion resistance and biocompatibility are needed: aerospace, medical devices, motorsport and chemical processing.

Designations and variants

  • Grade 5 (ASTM B265, B348) – standard Ti6Al4V; UNS R56400; EN 3.7165; DIN name TiAl6V4.
  • Grade 23 (ELI) – Extra Low Interstitial, with reduced oxygen and iron for higher toughness; UNS R56401, used for medical implants (ASTM F136).
  • Grade 2 – commercially pure titanium (not an alloy), lower strength and easier to machine; often compared with Grade 5.

For cross-references between standards see material designation equivalents. In the ISO 513 machinability classification, titanium belongs to group S (heat-resistant superalloys and titanium), see ISO material groups.

Key properties

PropertyTypical value (annealed Grade 5)
Densityabout 4.43 g/cm³
Tensile strength Rmabout 900–1100 MPa (ASTM minimum about 895 MPa)
Yield strength Rp0.2about 830–1000 MPa
Hardnessabout 30–36 HRC (roughly 300–350 HB)
Young's modulusabout 110–115 GPa
Thermal conductivityabout 6–7 W/(m·K)
Machinabilitydifficult; typically about 20–25 % of free-cutting steel

Hardness scales are explained in hardness scales.

Why titanium is hard to machine

  • Low thermal conductivity. Very little heat leaves with the chip, so it concentrates at the cutting edge. Edge temperature rises quickly, which limits cutting speed.
  • Chemical reactivity. At high temperature titanium tends to weld to the tool and form built-up edge, which leads to chipping.
  • Low elastic modulus. Thin walls and slender parts spring away from the tool, causing chatter and dimensional errors.
  • Flammability. Fine chips and dust can ignite, especially during grinding or dry machining. Water must not be used on burning titanium.

Machining guidelines

The values below are typical starting values; the tool manufacturer's data always takes priority.

OperationToolCutting speed VcNote
Milling (side milling)Coated solid carbide end millabout 40–80 m/minLow ae, larger ap; trochoidal toolpaths
TurningCarbide insert with sharp edgeabout 40–80 m/minGenerous coolant, ideally through-tool
DrillingCarbide drill with internal coolantabout 20–40 m/minContinuous feed, no dwelling
  • Use sharp, positive-rake edges and fine-grain carbide. PVD coatings such as TiAlN or AlTiN work well (see tool coatings).
  • Never dwell in the cut: rubbing without cutting work-hardens the surface and wears the edge quickly.
  • Keep the feed high enough: too low a feed per tooth causes rubbing instead of cutting.
  • Use generous emulsion coolant, ideally high-pressure (70 bar or more) through the tool.
  • Ensure rigid workholding and short tool overhang.
  • Enter the material gradually with arc or helical entries to avoid shock loading the edge.

Typical applications

  • Aerospace structural parts, fasteners and engine components (up to roughly 350–400 °C).
  • Medical implants, orthopaedic screws and dental implants (mostly Grade 23 ELI).
  • Motorsport and bicycle components, marine hardware.
  • Chemical processing equipment requiring resistance to chlorides.

Design tips for titanium parts

  • Internal radii. Specify internal corner radii as large as possible – at least slightly larger than the cutter radius. This prevents the cutter from wrapping into the corner and reduces load and chatter.
  • Wall thickness. Because of the low elastic modulus, thin walls (below about 1–1.5 mm) deflect. If they are necessary, machine them in steps, leaving support on the opposite side until the final pass.
  • Deep pockets and holes. Every extra millimetre of tool length reduces rigidity. Design deep features so that shorter tools can be used or the part can be machined from two sides.
  • Threads. Taps tend to seize in titanium. Thread milling is more reliable, or a slightly larger tap drill can be used where the standard allows, see taps.
  • Tolerances. Residual stress and springback make very tight tolerances expensive. Specify tight tolerances only on functional surfaces.

Surface and finishing

When machined correctly with sharp tools, titanium reaches a surface roughness of about Ra 0.8–1.6 µm without additional grinding (see surface roughness). An overheated surface turns yellow or blue – a sign that the cutting conditions are too aggressive or the tool is worn. On critical aerospace and medical parts such discolouration may be unacceptable, as it changes the properties of the surface layer. After machining, titanium is often passivated, anodised for colour or identification, or polished.

How to choose

If the part does not need high strength, consider Grade 2: it is easier to machine and cheaper. Choose Ti6Al4V when strength-to-weight ratio matters. For medical use choose the ELI variant with the appropriate certification. Compared with nickel alloys, Ti6Al4V is lighter and generally somewhat easier to machine, but it is not suited to very high service temperatures.

Suppliers of titanium milling and turning services can be found or requested on the CNC Pasaulis marketplace.

Frequently asked questions

What is the difference between Grade 5 and Grade 23 titanium?

Grade 23 (ELI) is the same Ti6Al4V alloy with reduced oxygen and iron. It is tougher and more resistant to cracking, so it is used for medical implants.

What cutting speed should be used to mill Ti6Al4V?

With coated carbide end mills a typical starting Vc is about 40–80 m/min. Always check specific values against the tool manufacturer's recommendations.

Can titanium be machined dry?

It is not recommended. Because of low thermal conductivity the edge overheats, and fine chips can ignite. Generous emulsion coolant is standard.

Why do titanium parts chatter during machining?

Titanium's elastic modulus is roughly half that of steel, so thin walls deflect. Rigid workholding, short tool overhang and lower radial engagement help.

Can Ti6Al4V be heat treated?

Yes, it can be annealed or solution treated and aged (STA) to increase strength. Most parts are machined in the annealed condition.