Nickel Alloys (Inconel 718, 625): Properties and Machining

Updated

In short

Nickel-based superalloys such as 718 (2.4668, UNS N07718) and 625 (2.4856, UNS N06625) retain strength and corrosion resistance at high temperatures. They are among the most difficult materials to machine: they work-harden rapidly, stay strong when hot and are abrasive. They are machined at low cutting speeds with a rigid setup and sharp coated carbide or ceramic tools.

Nickel alloys are nickel-based alloys containing chromium, iron, molybdenum, niobium and other elements. They are often called by the trade name Inconel, but alloys of the same composition are produced by various manufacturers and designated by standard numbers such as Alloy 718 or Alloy 625. These superalloys keep their strength up to about 650–700 °C and beyond, so they are used in gas turbines, aerospace, oil and gas, and chemical processing.

Common alloys and designations

AlloyEN no.EN / DIN nameUNSCharacteristics
Alloy 7182.4668NiCr19Fe19Nb5Mo3N07718Precipitation hardening, very high strength
Alloy 6252.4856NiCr22Mo9NbN06625Solid solution, excellent corrosion resistance
Alloy 6002.4816NiCr15FeN06600Oxidation resistant, lower strength
Alloy C-2762.4819NiMo16Cr15WN10276Resistant to aggressive media

For designation systems see material designation equivalents. In ISO 513 nickel alloys belong to group S, see ISO material groups.

Key properties

PropertyAlloy 718 (aged)Alloy 625 (annealed)
Densityabout 8.2 g/cm³about 8.4 g/cm³
Tensile strength Rmabout 1240–1450 MPaabout 830–1000 MPa
Hardnessabout 36–44 HRCabout 175–240 HB
Thermal conductivityabout 11 W/(m·K)about 10 W/(m·K)
Machinabilityvery difficult (about 10–15 % of free-cutting steel)very difficult, strong work hardening

Alloy 718 is often supplied solution annealed (around 25–30 HRC or lower) and aged after rough machining. For heat treatment conditions see heat treatment.

Why nickel alloys are hard to machine

  • Work hardening. The surface layer becomes considerably harder after cutting. A following pass that is too shallow cuts into already hardened material.
  • Hot strength. The material does not soften in the cutting zone, so cutting forces and edge temperatures are very high.
  • Low thermal conductivity. Heat accumulates at the edge, so cutting speeds must be low.
  • Abrasive carbides and intermetallic phases. These cause rapid notch wear at the depth-of-cut line.

Machining guidelines

The values below are typical starting values; the tool manufacturer's data takes priority.

OperationToolVc, m/min
TurningPVD-coated carbide insertabout 30–60
Rough turningCeramic insert (SiAlON, whisker)about 150–300
MillingCoated solid carbide end millabout 20–50
DrillingCarbide drill with internal coolantabout 10–25
  • Use sharp but reinforced edges and PVD coatings (e.g. TiAlN, AlTiN), see tool coatings.
  • Depth of cut and feed per tooth must exceed the work-hardened layer – avoid rubbing and very light passes.
  • Vary the depth of cut between passes or use round inserts to spread notch wear.
  • Ceramics are for roughing only, usually without coolant or as the manufacturer specifies; finishing is done with carbide.
  • Ensure very rigid workholding and short tool overhang; vibration quickly breaks the edge.
  • Use generous coolant, ideally high-pressure through the tool.
  • When milling, use climb milling and trochoidal toolpaths with low radial engagement.

Typical applications

  • Gas turbine discs, shafts, casings and fasteners (718).
  • Rocket and aero-engine components.
  • Marine, oil and gas equipment and heat exchangers (625, C-276).
  • Exhaust systems, furnace and heat treatment equipment (600).

Design and process tips

  • Stock condition. State the stock condition (annealed, aged) and the material specification, e.g. AMS or EN, on the drawing and order. Both the cutting conditions and the final part properties depend on it.
  • Roughing and finishing. Leave an even finishing allowance so that the finishing tool always cuts beneath the work-hardened layer rather than within it.
  • Threads. Taps often break in nickel alloys. Thread milling is more reliable; for small threads use dedicated taps and tight control of the tap drill diameter, see taps.
  • Internal radii and depth. As with titanium, larger internal radii and shorter tools greatly extend tool life.
  • Surface integrity. Aerospace parts may have requirements on white layer, residual stress and microcracks. A worn tool can damage the surface layer, so tool change intervals are set conservatively.

Economics

Nickel alloys cost several times more per kilogram than stainless steel, and machining times are longer because of low cutting speeds. It therefore pays to design parts so that as little material as possible is removed: use near-net-shape forgings, castings or additively manufactured blanks, and apply CNC machining to functional surfaces. Tooling costs make up a significant share of the production cost of such parts.

How to choose

For maximum strength up to about 650 °C choose Alloy 718. Where corrosion resistance and weldability matter most, choose Alloy 625 or C-276. If temperature and corrosion are not extreme, consider stainless steel or titanium alloy, which are generally easier to machine and cheaper. Nickel alloy parts are expensive, so agree on stock condition, tolerances and certification in advance.

Nickel alloy machining services can be found or requested on the CNC Pasaulis marketplace.

Frequently asked questions

Are Inconel and Alloy 718 the same?

Inconel is a trade name, while Alloy 718 is the standard alloy designation (2.4668, UNS N07718). Alloy 718 from different producers meets the same standards.

What cutting speed is used for turning Inconel 718?

With coated carbide inserts a typical starting Vc is about 30–60 m/min, and for roughing with ceramic inserts about 150–300 m/min. Check values against the tool manufacturer's data.

Why do tools fail quickly in nickel alloys?

Common causes are work hardening, passes that are too light, vibration and notch wear at the depth-of-cut line. A rigid setup and adequate feed help.

Is Alloy 718 machined before or after ageing?

It is often rough machined in the solution-annealed condition, then aged and finish machined. The exact sequence depends on the drawing requirements.

How do nickel alloys differ from titanium?

Nickel alloys are almost twice as heavy but retain strength at higher temperatures. They are usually machined at even lower cutting speeds than titanium.