Polyamide PA6: Properties, Moisture and CNC Machining

Updated

In short

Polyamide PA6 (nylon 6) is a tough, wear-resistant engineering plastic widely used for gears, rollers and sliding parts. Its main drawback is moisture absorption, which changes dimensions and mechanical properties and must be considered in design and machining.

Polyamide PA6 (nylon 6) is a semi-crystalline engineering thermoplastic with high toughness and good impact and wear resistance. It is produced by extrusion (PA6E) or cast from monomer (PA6G, cast nylon) when large rods, plates and tubes are required.

Grades

  • PA6 (extruded) – general purpose, toughest, highest moisture uptake.
  • PA6G (cast) – higher crystallinity, stiffness and wear resistance, lower internal stress, very large blanks possible.
  • PA6G with oil or MoS₂ – self-lubricating grades for sliding parts.
  • PA66 – closely related, with a higher melting point and stiffness.
  • PA6 GF30 – glass-filled, stiffer but more abrasive on tools.

Key properties

PropertyDryConditioned (approx. 50 % RH)
Density1.13–1.15 g/cm³
Tensile strength70–85 MPa40–60 MPa
Tensile modulus2.8–3.5 GPa1.0–1.8 GPa
Moisture absorptionapprox. 2.5–3.5 % at 50 % RH, up to approx. 9 % saturated in water
Melting pointapprox. 215–220 °C
Continuous service temperatureapprox. −40 to +80…100 °C
MachinabilityGood, but chips are long and stringy

Values are indicative and grade-dependent; refer to the supplier's data sheet for exact figures.

Typical applications

  • Gears, sprockets, rollers and pulleys.
  • Sliding bushings, guides and wear plates.
  • Conveyor and packaging machinery parts.
  • Guide rings for lifting equipment and hydraulic cylinders.

Moisture and dimensions

The defining feature of PA6 is moisture absorption. As it takes up water it swells (up to about 2–3 % in volume when saturated), becomes softer and tougher, and loses strength and stiffness. Therefore:

  • design precision parts with wider tolerances than for POM;
  • give bushings extra running clearance so they do not seize in humid conditions;
  • measure parts knowing the conditioning state of the material;
  • in wet or underwater service, consider POM, filled PA6G or UHMW-PE.

CNC machining tips

  • Tools: very sharp carbide or HSS tools with a large positive rake; single-flute end mills for plastics work well.
  • Chips: PA6 forms long, tough chips that wrap around the tool and workpiece in turning. Use chip breakers, interrupted feed and compressed air.
  • Cutting speed: a typical starting value for milling with carbide is about 200–500 m/min, with enough feed that the tool cuts rather than rubs; the tool manufacturer's data takes priority.
  • Cooling: compressed air or water-based coolant; overheating causes melting and burrs.
  • Burrs: PA6 tends to leave thin burrs on edges – plan chamfers and a final pass with a sharp tool.

Turning and stock forms

Polyamide is frequently turned – bushings, rollers, pulleys and guide rings are made from rod and tube. Sharp aluminium-type inserts with a positive rake and polished rake face are suitable. A typical starting feed is about 0.1–0.4 mm/rev, and cutting speed can be high, limited mainly by workpiece heating and chip control. The tool manufacturer's data takes priority. Long blanks need tailstock support because PA6 is flexible.

Cast PA6G blanks can be very large – plates several hundred millimetres thick, and rods and tubes up to several hundred millimetres in diameter. They usually contain less internal stress than extruded stock, so large parts distort less after machining. For precision parts, rough machining with allowance, a rest period and final finishing are still recommended.

Managing moisture in practice

Some producers condition PA6 parts after machining – keeping them in water or a humid environment so the material reaches equilibrium moisture and becomes tougher. In other cases parts are kept dry to preserve dimensions. It is important that the drawing clearly states the condition in which dimensions are inspected. The bore of bushings is often made larger to allow for swelling from moisture and temperature; specific clearances are given in the material producers' design recommendations.

How to choose

Choose PA6G for large, loaded, wearing parts where toughness and cost matter. Choose extruded PA6 for smaller general-purpose parts. If precise dimensions in humid conditions are required, POM is the better choice; for high temperatures, use PEEK.

Suitable polyamide machining services can be found or requested on the CNC Pasaulis marketplace.

Frequently asked questions

What is the difference between PA6 and cast nylon PA6G?

Both are the same polymer type, but PA6G is cast from monomer rather than extruded. It is somewhat stiffer, more wear resistant, lower in internal stress and available in very large sizes.

How much moisture does PA6 absorb?

About 2.5–3.5 % at 50 % relative humidity and up to about 9 % when saturated in water. This changes dimensions and reduces stiffness.

How do I avoid long chips when turning PA6?

Use sharp inserts with a chip breaker, interrupted feed and compressed air to clear chips. This reduces chip wrapping.

Is PA6 good for gears?

Yes, PA6 and PA6G are among the most popular plastic gear materials thanks to their toughness, noise damping and wear resistance.

When should I choose POM instead of PA6?

When precise, stable dimensions in humid conditions and easy machining are important. PA6 is better when impact resistance and large blank sizes matter more.