Powder Coating: Process, Film Thickness, Pre-treatment and Standards
Updated
Powder coating is a finishing process in which dry paint powder is sprayed electrostatically onto grounded metal and then melted and cured in an oven, typically at 160–200 °C. It produces a tough coating about 60–120 µm thick, widely used on steel and aluminium products.
Powder coating is an organic coating method that uses dry powder made of resin, pigments and additives instead of liquid paint. The powder adheres electrostatically to the grounded part and in a curing oven melts, flows and cross-links chemically. The process releases almost no solvents, and overspray can often be recovered and reused.
Process steps
- Surface pre-treatment – degreasing, rinsing, conversion coating (phosphating or chrome-free processes) or abrasive blasting.
- Drying – removing moisture before coating.
- Masking – covering threads, holes and contact surfaces with plugs or tape.
- Electrostatic spraying – the gun charges the powder (corona or tribo charging).
- Curing – in an oven, typically 160–200 °C for 10–20 min at part temperature (per powder manufacturer data).
- Cooling and inspection – thickness, adhesion and appearance checks.
Powder types
| Type | Properties | Use |
|---|---|---|
| Polyester | Good UV and weather resistance | Outdoor products, facades, fencing |
| Epoxy | Excellent chemical resistance and adhesion, but chalks under UV | Indoor equipment, primers |
| Epoxy-polyester (hybrid) | Compromise, economical | Indoor products, furniture, appliances |
| Polyurethane | Smooth finish, chemical resistance | Equipment, machine parts |
Film thickness and dimensions
| Coating | Typical thickness |
|---|---|
| Single coat | ~60–120 µm |
| Primer + topcoat | ~120–200 µm and more |
This is much thicker than anodizing or zinc electroplating, so threads, precision holes and fitting surfaces are normally masked. Coverage is thinner on edges and in corners (the Faraday cage effect makes deep internal corners hard to coat).
Surface pre-treatment
Coating durability depends mostly on pre-treatment. Steel is abrasive blasted (e.g. to cleanliness grade Sa 2½ per ISO 8501-1) and/or zinc phosphated. Aluminium is degreased, etched and conversion coated. The oxide film left on edges after oxygen-assisted laser cutting can impair adhesion and is therefore removed (see laser cutting).
Colours and gloss
- Colour is usually specified from the RAL chart (e.g. RAL 9005 jet black, RAL 7016 anthracite grey).
- Gloss levels: matt, semi-matt, semi-gloss, gloss – measured in gloss units at 60°.
- Textures: smooth, fine texture, wrinkle, metallic.
Corrosion protection
Atmospheric corrosivity for steel is classified in ISO 12944-2 into categories C1–C5 and CX. For aggressive environments (e.g. C4–C5) a duplex system – hot-dip galvanizing plus powder coating – is often used, giving longer protection than either coating alone. For architectural aluminium, quality requirements are defined for example by Qualicoat specifications.
What to state in a request
- RAL colour, gloss and texture.
- Service environment (indoor, outdoor, corrosivity category).
- Required film thickness or system (primer + topcoat).
- Surfaces to mask, threads and grounding points.
- Whether racking marks are acceptable and where.
Design tips
- Provide a hanging hole or point that is not visible.
- Avoid closed cavities without drainage – pre-treatment chemicals can remain trapped.
- Round edges – coating on sharp edges is thinner and damaged more easily.
Common defects and causes
| Defect | Typical cause |
|---|---|
| Orange peel | Excessive film build, incorrect cure or powder properties |
| Pinholes, blisters | Outgassing from castings or galvanized steel; pre-heating helps |
| Poor adhesion | Insufficient cleaning, oxides, oil |
| Uncoated internal corners | Faraday cage effect |
| Colour mismatch | Different powder batches, overbaking |
Film thickness is usually measured with a magnetic or eddy-current gauge and adhesion by the cross-cut test per ISO 2409. These tests can be specified in the order as acceptance criteria.
Powder coating and metal fabrication services can be found or requested on the CNC Pasaulis marketplace.
Frequently asked questions
How thick is a powder coating?
Usually 60–120 µm for a single coat, and 120–200 µm or more for two-coat systems.
At what temperature is powder coating cured?
Typically 160–200 °C for about 10–20 minutes at part temperature; the exact schedule is given by the powder manufacturer.
Do threads need masking for powder coating?
Yes, the thick film would fill the thread. Threads and precision surfaces are covered with plugs or tape.
Can galvanized steel be powder coated?
Yes, this is known as a duplex system. It requires proper preparation of the zinc surface for good adhesion.
How is colour specified?
Usually by RAL number, together with gloss level and texture.
Looking for someone to do this job? Find a manufacturer on the marketplace or post a request.
Services offered I need a service