Sinker EDM: Electrodes, Accuracy and Applications

Updated

In short

Sinker EDM is a process in which a shaped graphite or copper electrode, immersed in dielectric oil, erodes its negative form into an electrically conductive workpiece using spark discharges. It produces blind cavities, deep narrow ribs and sharp internal corners in hardened steel, especially in moulds and dies.

Sinker EDM (ram EDM, die-sinking EDM) is electrical discharge machining in which the tool is a pre-made electrode whose shape is reproduced in the workpiece. Unlike wire EDM, it can produce blind, enclosed cavities.

Working principle

The electrode and workpiece are submerged in a dielectric fluid – usually a dedicated hydrocarbon oil. A small gap is maintained between them, in which the generator creates thousands of sparks per second. Each spark melts a tiny amount of material, which the dielectric flushes away. The electrode gradually sinks (in Z) or moves in an orbital path until the required depth and shape are reached.

The workpiece must be electrically conductive. Hardness has practically no effect, so already hardened tool steel is often eroded (see heat treatment).

Electrode materials

MaterialPropertiesTypical use
GraphiteEasy and fast to mill, low wear in roughing, lightweightLarge and complex electrodes, moulds
Electrolytic copperGood finishing surface but harder to machine and heavierFine features, polished surfaces
Copper–tungstenVery low wear, expensiveEroding carbide, fine details

Electrodes are usually made by CNC milling. They are made undersize by the spark gap, which per side typically ranges from a few hundredths to a few tenths of a millimetre depending on the settings. At least two electrodes – roughing and finishing – are common.

Surface finish and accuracy

ModeTypical RaNotes
Roughing~3–12 µmHigh removal rate, matte texture
Semi-finishing~1–3 µmIntermediate stage
Finishing~0.2–0.8 µmSlow, often with copper electrode

Typical dimensional tolerance is ±0.01–0.02 mm, tighter around ±0.005 mm depending on electrode accuracy and process. The eroded surface has a characteristic matte texture that is sometimes used directly as a decorative mould finish; some textures are standardised (e.g. the VDI 3400 scale).

Applications

  • Cavities, ribs and deep narrow slots in die-casting and injection moulds.
  • Sharp internal corners impossible with an end mill.
  • Cavities in hardened steel and carbide.
  • Small hole drilling by EDM (separate fast hole EDM machines with tube electrodes), e.g. start holes for wire EDM.
  • Helical or complex profiles using orbital or rotating electrode motion.

Limitations

  • Slow material removal, especially when finishing.
  • Electrodes must be made – extra time and cost.
  • A recast and heat-affected layer forms on the surface; for critical uses it is removed by polishing or gentle settings.
  • Conductive materials only.

Design tips

  • Where possible, allow a radius in internal corners so the cavity can be milled and EDM is not needed.
  • Specify the required texture or surface roughness on the drawing.
  • Deep, narrow ribs in moulds are a typical sinker EDM case.

Process parameters and flushing

Sinker EDM productivity and quality are governed by generator settings: pulse duration, current, pause and polarity. Longer, stronger pulses remove material faster but give a rougher surface and more electrode wear. The process is therefore split into several stages with progressively gentler settings.

Flushing is critical – eroded particles must be removed from the gap, otherwise unstable discharges and damage to electrode or workpiece occur. Pressure or suction flushing through electrode holes, periodic electrode retraction and orbiting are used. Orbiting (moving the electrode in a circle or contour) also allows one electrode to reach different sizes and treats side walls more evenly.

The number of electrodes and their undersize depend on the required finish, so a request should state not only dimensions but also the required roughness or texture.

EDM services can be found or requested on the CNC Pasaulis marketplace.

Frequently asked questions

What is the difference between sinker and wire EDM?

Wire EDM cuts through-profiles with a thin wire, while sinker EDM erodes blind cavities with a shaped electrode. Both work only on conductive materials.

What are EDM electrodes made of?

Usually graphite or electrolytic copper, less often copper–tungsten. They are normally produced by CNC milling.

Why is the electrode smaller than the cavity?

A spark gap always remains between electrode and workpiece, so the cavity ends up larger than the electrode. The electrode is undersized by this gap.

Can hardened steel be eroded?

Yes, hardness has almost no effect on the process. Moulds are therefore often hardened first and then eroded.