CNC Grinding: Surface, Cylindrical and Centreless Grinding
Updated
CNC grinding is an abrasive finishing process in which a rotating grinding wheel removes a very thin layer of material. It achieves IT5–IT6 tolerances and Ra 0.1–0.4 µm, so it is used for hardened shafts, bearing seats, cutting tools and precision flat surfaces.
Grinding is machining with an abrasive tool (grinding wheel) whose many hard grains act as microscopic cutting edges. CNC grinding machines control wheel and workpiece motion and wheel dressing, making the process repeatable and highly accurate. Grinding is most often applied to parts already hardened by heat treatment.
Types of grinding
| Type | Workholding | Use |
|---|---|---|
| Surface grinding | Magnetic chuck | Flat surfaces, parallelism, tool plates, die components |
| External cylindrical grinding | Between centres or in a chuck | Shafts, bearing seats, pins |
| Internal cylindrical grinding | Chuck | Bores, bushings, bearing housings |
| Centreless grinding | Supported on a work rest blade between grinding and regulating wheels | High-volume pins, rollers, bars |
| Profile grinding | Various | Threads, gears, profiles, die forms |
| Tool grinding | 5-axis tool and cutter grinders | Manufacturing and resharpening carbide end mills and drills |
Achievable accuracy
| Parameter | Standard grinding | Precision grinding |
|---|---|---|
| Dimensional tolerance | IT6 (e.g. Ø30: 13 µm band) | IT5 and tighter |
| Surface roughness Ra | 0.2–0.8 µm | 0.05–0.2 µm |
| Roundness | ~2–5 µm | ~1 µm |
| Flatness | ~5 µm over 100 mm | ~1–2 µm |
Values are indicative and depend on the machine, material, thermal stability and measuring conditions. For tolerance grades see ISO tolerances and fits; for roughness see surface roughness.
Grinding wheels
- Aluminium oxide – steels, including hardened steels.
- Silicon carbide – cast iron, non-ferrous metals, non-metals.
- Cubic boron nitride (CBN) – hardened steels, long life and stable size.
- Diamond – carbide, ceramics, glass; unsuitable for steel at high speed due to chemical wear.
The wheel specification states abrasive, grit size, grade (bond strength), structure and bond type (e.g. vitrified, resin, metal). The wheel is periodically dressed to restore form and sharpness.
Process considerations
- Grinding allowance – usually 0.1–0.3 mm on diameter (depending on size and heat treatment distortion); too little may not clean up distortion, too much prolongs the process.
- Heat – wrong parameters or coolant cause grinding burn, surface tempering and micro-cracks. Critical parts are checked for burn (e.g. by etching).
- Coolant – cutting fluid cools the zone and flushes away swarf.
When grinding is needed
- When a surface requires IT6 or tighter and/or Ra below about 0.4 µm.
- When the part is hardened beyond what can be economically turned or milled (see hardness scales).
- Bearing, seal and sliding surfaces, gauges, die and mould components.
Note: hardened steel up to about 60–65 HRC can in some cases be hard-turned with CBN inserts – an alternative to grinding where tolerance and surface requirements allow.
What to specify on the drawing
Clearly mark ground surfaces with tolerances and roughness, state hardness after heat treatment and geometric tolerances (roundness, runout, parallelism). See technical drawings for CNC machining.
Grinding or hard turning
| Criterion | Grinding | Hard turning (CBN) |
|---|---|---|
| Tolerance | IT5–IT6 and tighter | Often IT6–IT7 |
| Roughness Ra | Down to ~0.1 µm | Often ~0.2–0.8 µm |
| Flexibility | Wheel must be dressed to the profile | Contours programmed flexibly |
| Cooling | Coolant required | Often possible dry |
| Typical use | Bearing seats, long surfaces, very precise flats | Short complex contours, gear bores |
The choice depends on part geometry, requirements and batch size. The two are often combined: hard turning removes most of the stock and critical surfaces are ground.
Grinding services can be found or requested on the CNC Pasaulis marketplace.
Frequently asked questions
What accuracy does grinding achieve?
Typically IT6 tolerances and Ra 0.2–0.8 µm, and IT5 with Ra down to 0.05–0.2 µm in precision grinding.
Why grind after hardening?
Hardening distorts and hardens the part. Grinding removes the distortion and produces final dimensions in the hard material.
What is centreless grinding?
External cylindrical grinding where the part is not held between centres but supported on a blade between the grinding and regulating wheels. It is very productive in series production.
How much stock is left for grinding?
Usually 0.1–0.3 mm on diameter, depending on part size and heat treatment distortion.
What is grinding burn?
Surface overheating caused by incorrect parameters, leading to tempering, discolouration or micro-cracks. It reduces part fatigue strength.