Hardness conversion HRC ↔ HB ↔ HV
In short
Pick a scale and enter a value to get the equivalents. Conversion is approximate, for unalloyed and low-alloy steel (based on ASTM E140 / ISO 18265 tables, linear interpolation). E.g. 40 HRC ≈ 392 HV ≈ 371 HB.
Rm ≈ 3.2 × HV (MPa, approximate, steel only)
Hardness conversion table (steel, approximate)
| HRC | HV | HB | Rm ≈ MPa |
|---|---|---|---|
| – | 100 | 95 | 320 |
| – | 140 | 133 | 450 |
| – | 180 | 171 | 575 |
| – | 220 | 209 | 705 |
| 20 | 238 | 226 | 760 |
| 25 | 266 | 253 | 850 |
| 30 | 302 | 286 | 965 |
| 35 | 345 | 327 | 1 105 |
| 40 | 392 | 371 | 1 255 |
| 45 | 446 | 421 | 1 425 |
| 50 | 513 | 481 | 1 640 |
| 55 | 595 | 560 | 1 905 |
| 60 | 697 | 654 | – |
| 65 | 832 | – | – |
| 68 | 940 | – | – |
CNC calculators
See all →Frequently asked questions
How hard is hardened steel in HRC?
Hardened tool steel is often 55–62 HRC; quenched and tempered structural steel (e.g. 42CrMo4) is around 28–40 HRC.
Can hardness be converted exactly?
No – the scales measure differently, so conversion is always approximate. For acceptance testing, use the scale specified on the drawing.
At what hardness does milling get difficult?
Above ~45 HRC special carbide tools and lower cutting data are needed; above ~55 HRC grinding or EDM is often chosen.